热处理工艺对690 MPa级高强钢屈强比的影响

    Effect of Heat Treatments on Yield Strength Ratio of 690 MPa Grade High Strength Steel

    • 摘要: 研究热处理工艺对690 MPa级高强钢的屈强比的影响,并采用金相显微镜对其相应工艺的显微组织进行分析。结果表明:采用860℃×50min淬火+610℃×50min回火工艺,钢板的力学性能都满足标准GB/T 16270-2009对690 MPa级高强钢的要求,同时屈强比降低到0.92,其基体组织为回火索氏体+针片状铁素体。经过“临界温度淬火+高温短时回火”工艺处理后,可以大幅降低690 MPa级高强钢的屈强比,同时保持良好强度,不降低或者稍微降低韧性和塑性。

       

      Abstract: The eff ect of heat treatment process on the yield strength ratio of 690 MPa grade high strength steel was studied. The microstrueture of the corresponding process was analyzed by metallographic micrescope. The results show that,using 860℃×50 min quenching and 610 ℃×50 min tempering process, the mechanical properties of the steel plate meet the standard GB/T 16270-2009 requirements for 690 MPa grade high strength steel. At the same time, the yield strength ratio decreases to 0.92, the matrix microstructure is tempered sorbite+needle flake ferrite. After "critical temperature quenching and high temperature short time tempering" process, the yield strength ratio of 690 MPa grade high stre ngth steel can be greatly reduced, while maintaining good strength, not reducing or slightly reducing the toughness and plasticity.

       

    /

    返回文章
    返回