Research on Corrosion Behavior of Al2O3 and Al2O3-MnS Inclusions in Non-oriented Silicon Steel
-
-
Abstract
The annealed samples of non-oriented silicon steel were used for in-situ corrosion experiments, and the surface corrosion morphology of the samples was characterized by OM, SEM, EDS and Raman spectroscopy. The results show that the corrosion of non-oriented silicon steel originates from the localized corrosion of inclusions, including metal oxide inclusions Al2O3 and metal oxysulfide inclusions Al2O3-MnS. During the initial corrosion of non-oriented silicon steel, the corrosion products in the circular rust spots are mainly γ-FeOOH and α-Fe2O3, and the content of γ-FeOOH is higher than that of α-Fe2O3.As the color of the corrosion products deepens, the content of α-Fe2O3 gradually increases.
-
-